PA6 GF30

Alternative and trade names
PA6-GF30
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 6 (PA6) reinforced with 30% glass fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.35 g/cm³

Show Supplier Material materials with Density of 1.35 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ASTM D638

Flexural modulus

23.0 °C

7.8 GPa

Show Supplier Material materials with Flexural modulus of 7.8 GPa

ASTM D790

Flexural strength

23.0 °C

220 MPa

Show Supplier Material materials with Flexural strength of 220 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

12 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 12 J/m

ASTM D256

Tensile strength

23.0 °C

181 MPa

Show Supplier Material materials with Tensile strength of 181 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

203 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 203 °C

ASTM D648

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ASTM D2117

Flammability

UL 94 HB (1.6mm)

Technological properties

Property
Application areas

Auto parts, power tools, wipers

Fillers

30% Glass Fiber