General

PropertyTemperatureValueComment

Density

23.0 °C

1.39 g/cm³

Show Supplier Material materials with Density of 1.39 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1 - 3 %

Show Supplier Material materials with Elongation of 1 - 3 %

ASTM D638

Flexural modulus

23.0 °C

17.2 GPa

Show Supplier Material materials with Flexural modulus of 17.2 GPa

ASTM D790

Flexural strength

23.0 °C

305 MPa

Show Supplier Material materials with Flexural strength of 305 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

640 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 640 J/m

ASTM D256

Tensile strength

23.0 °C

234 MPa

Show Supplier Material materials with Tensile strength of 234 MPa

ASTM D638

Tear strength

97.0

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

216 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 216 °C

ASTM D648

Melting point

345 °C

Show Supplier Material materials with Melting point of 345 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.1 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.1 - 0.2 %

Technological properties

Property
Application areas

Steaming tray, bell-shaped cover, microwave bowl, oven utensils

Fillers

30% Carbon Fiber