PPS GF20

Alternative and trade names
PPS-GF20
Want to keep this datasheet? Save it now in your required format

Description

Polyphenylene Sulfide (PPS) reinforced with 20% glass fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.51 g/cm³

Show Supplier Material materials with Density of 1.51 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

11.4 GPa

Show Supplier Material materials with Flexural modulus of 11.4 GPa

ASTM D790

Flexural strength

23.0 °C

170 MPa

Show Supplier Material materials with Flexural strength of 170 MPa

ASTM D790

Hardness, Shore D

23.0 °C

84 [-]

Show Supplier Material materials with Hardness, Shore D of 84 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

80 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 80 J/m

ASTM D256

Tensile strength

23.0 °C

125 MPa

Show Supplier Material materials with Tensile strength of 125 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

264 °C

Show Supplier Material materials with Heat deflection temperature of 264 °C

ASTM D648

Technological properties

Property
Application areas

Automotive bumpers, Automotive applications, Automotive exterior parts

Fillers

20% Glass Fiber