PA6 Toughened

Alternative and trade names
PA6-I
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 6 (PA6) is an impact modified grade

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.02 g/cm³

Show Supplier Material materials with Density of 1.02 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

35 %

Show Supplier Material materials with Elongation of 35 %

Minimum, ASTM D638

Flexural modulus

23.0 °C

1.8 GPa

Show Supplier Material materials with Flexural modulus of 1.8 GPa

ASTM D790

Flexural strength

23.0 °C

60 MPa

Show Supplier Material materials with Flexural strength of 60 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

60 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 60 J/m

ASTM D256

Tensile strength

23.0 °C

48 MPa

Show Supplier Material materials with Tensile strength of 48 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

130 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 130 °C

ASTM D648

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ASTM D2117

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

ASTM D257

Technological properties

Property
Additives

Toughening Additive

Application areas

Wheels, electrical shell, automotive parts, rollers, sports equipment