Description

Polyamide 6 (PA6) is a brominated flame retardant Virgin Grade

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.33 g/cm³

Show Supplier Material materials with Density of 1.33 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

3 GPa

Show Supplier Material materials with Flexural modulus of 3 GPa

ASTM D790

Flexural strength

23.0 °C

82 MPa

Show Supplier Material materials with Flexural strength of 82 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

7.5 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 7.5 J/m

ASTM D256

Tensile strength

23.0 °C

55 MPa

Show Supplier Material materials with Tensile strength of 55 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

220 °C

Show Supplier Material materials with Heat deflection temperature of 220 °C

ASTM D648

Flammability

UL 94 V0 (1.6mm)

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.2 - 1.3 %

Show Supplier Material materials with Shrinkage of 1.2 - 1.3 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Additives

Brominated flame retardant Additive