PA66 GF25 V0

Alternative and trade names
PA66-GF25 FR
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 66 (PA66), reinforced with 25% glass fiber, is a brominated flame retardant Virgin Grade.

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Supplier Material materials with Density of 1.42 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

6 %

Show Supplier Material materials with Elongation of 6 %

ASTM D638

Flexural modulus

23.0 °C

7.22 GPa

Show Supplier Material materials with Flexural modulus of 7.22 GPa

ASTM D790

Flexural strength

23.0 °C

167 MPa

Show Supplier Material materials with Flexural strength of 167 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

18 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 18 J/m

ASTM D256

Tensile strength

23.0 °C

136 MPa

Show Supplier Material materials with Tensile strength of 136 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

245 °C

Show Supplier Material materials with Heat deflection temperature of 245 °C

ASTM D648

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ASTM D2117

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 - 0.4 %

Show Supplier Material materials with Shrinkage of 0.3 - 0.4 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Additives

Brominated flame retardant

Fillers

25% Glass Fiber