Description

Polycarbonate (PC) is a UV Stabilized Grade

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

2.4 GPa

Show Supplier Material materials with Flexural modulus of 2.4 GPa

ASTM D790

Flexural strength

23.0 °C

92 MPa

Show Supplier Material materials with Flexural strength of 92 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

750 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 750 J/m

ASTM D256

Tensile strength

23.0 °C

62 MPa

Show Supplier Material materials with Tensile strength of 62 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

130 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 - 0.7 %

Show Supplier Material materials with Shrinkage of 0.5 - 0.7 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Additives

Anti-UV