POM GF30

Alternative and trade names
POM-GF30
Want to keep this datasheet? Save it now in your required format

Description

Polyoxymethylene (POM), reinforced with 30% glass fiber, is both weather and UV resistant

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.63 g/cm³

Show Supplier Material materials with Density of 1.63 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

8.27 GPa

Show Supplier Material materials with Flexural modulus of 8.27 GPa

ASTM D790

Flexural strength

23.0 °C

152 MPa

Show Supplier Material materials with Flexural strength of 152 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

53 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m

ASTM D256

Thermal

PropertyValueComment

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

ASTM D2117

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Technological properties

Property
Fillers

30% Glass Fiber