Description

Acrylonitrile Butadiene Styrene (ABS) reinforced with 10% carbon fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1 %

Show Supplier Material materials with Elongation of 1 %

ASTM D638

Flexural modulus

23.0 °C

7.58 GPa

Show Supplier Material materials with Flexural modulus of 7.58 GPa

ASTM D790

Flexural strength

23.0 °C

117 MPa

Show Supplier Material materials with Flexural strength of 117 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

53 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m

ASTM D256

Tensile strength

23.0 °C

82.7 MPa

Show Supplier Material materials with Tensile strength of 82.7 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

110 °C

Show Supplier Material materials with Heat deflection temperature of 110 °C

ASTM D648

Flammability

UL 94 HB (1.6mm)

Technological properties

Property
Fillers

10% Carbon Fiber