Description

40% Glass Fiber Reinforced Polyamide 6 (PA6-GF40)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.47 g/cm³

Show Supplier Material materials with Density of 1.47 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2.5 %

Show Supplier Material materials with Elongation of 2.5 %

ASTM D638

Flexural modulus

23.0 °C

9.65 GPa

Show Supplier Material materials with Flexural modulus of 9.65 GPa

ASTM D790

Flexural strength

23.0 °C

228 MPa

Show Supplier Material materials with Flexural strength of 228 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

130 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 130 J/m

ASTM D256

Tensile strength

23.0 °C

183 MPa

Show Supplier Material materials with Tensile strength of 183 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ASTM D648

Melting point

215 °C

Show Supplier Material materials with Melting point of 215 °C

ASTM D2117

Flammability

UL94 HB

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.00E+15 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+15 Ω·m

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Application areas

Scooter, bearing, fender, bumper, water tank, car handle, bicycle, fuel tank, frame, refrigerator housing, etc

Fillers

40% Glass Fiber