PP GF40

Alternative and trade names
PP-GF40
Want to keep this datasheet? Save it now in your required format

Description

40% Glass Fiber Reinforced Polypropylene (PP-GF40)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

ASTM D638

Flexural modulus

23.0 °C

6.89 GPa

Show Supplier Material materials with Flexural modulus of 6.89 GPa

ASTM D790

Flexural strength

23.0 °C

93 MPa

Show Supplier Material materials with Flexural strength of 93 MPa

Hardness, Shore D

23.0 °C

112 [-]

Show Supplier Material materials with Hardness, Shore D of 112 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

96 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 96 J/m

ASTM D256

Tensile strength

23.0 °C

68.5 MPa

Show Supplier Material materials with Tensile strength of 68.5 MPa

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

140 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C

ASTM D648

Melting point

163 °C

Show Supplier Material materials with Melting point of 163 °C

ASTM D2117

Flammability

UL94 HB

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Electrical resistivity

23.0 °C

3.00E+16 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.00E+16 Ω·m

Technological properties

Property
Application areas

car bumper,Tube, switch box, fan motor cover, refrigerator back cover, motor support cover, TV shell, refrigerator lining, drawer, soymilk machine cover, electric kettle shell etc

Fillers

40% Glass Fiber