30% Glass Fiber Reinforced Polyphenylene Sulfide (PPS-GF30)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.56 g/cm³

Show Supplier Material materials with Density of 1.56 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.6 %

Show Supplier Material materials with Elongation of 1.6 %

ASTM D638

Flexural modulus

23.0 °C

12 GPa

Show Supplier Material materials with Flexural modulus of 12 GPa

ASTM D790

Flexural strength

23.0 °C

180 MPa

Show Supplier Material materials with Flexural strength of 180 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

78 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 78 J/m

ASTM D256

Tensile strength

23.0 °C

130 MPa

Show Supplier Material materials with Tensile strength of 130 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

255 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 255 °C

ASTM D648

Melting point

295 °C

Show Supplier Material materials with Melting point of 295 °C

ASTM D2117

Flammability

UL94 V0

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Surface resistivity

23.0 °C

1.00E+16 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Application areas

Automobiles, electronic appliances and home appliances,Connector, switch, DVD laser head, coil frame, gearbox, circuit board, lamp holder, reflector lamp cup and bracket, throttle body, junction box, oil pump impeller, valve body, LED lamp housing, thermal circuit board, heat dissipation element etc

Fillers

30% Glass Fiber