TPU GF20

Alternative and trade names
TPU-GF20
Want to keep this datasheet? Save it now in your required format

Description

20% Glass Fiber Reinforced Thermoplastic Polyurethane (TPU-GF40)

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

85 %

Show Supplier Material materials with Elongation of 85 %

ASTM D638

Hardness, Shore D

23.0 °C

110 [-]

Show Supplier Material materials with Hardness, Shore D of 110 [-]

ASTM D785

Tensile strength

23.0 °C

47 MPa

Show Supplier Material materials with Tensile strength of 47 MPa

ASTM D638

Flexural modulus

ASTM D790

Tear strength

47.0

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

178 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 178 °C

ASTM D648

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

ASTM D955(GB15585), Molding Shrinkage

Technological properties

Property
Application areas

Electronic plugs, auto parts, mechanical parts, ships, aerospace, electronic housing etc

Fillers

20% Glass Fiber