General

PropertyTemperatureValueComment

Density

23.0 °C

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural strength

23.0 °C

42 MPa

Show Supplier Material materials with Flexural strength of 42 MPa

ASTM D790

Hardness, Shore D

23.0 °C

67 [-]

Show Supplier Material materials with Hardness, Shore D of 67 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

87 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 87 J/m

ASTM D256

Tensile strength

23.0 °C

27 MPa

Show Supplier Material materials with Tensile strength of 27 MPa

ASTM D638

Flexural modulus

ASTM D790

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

142 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 142 °C

ASTM D648

Melting point

125 °C

Show Supplier Material materials with Melting point of 125 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.8 - 1 %

Show Supplier Material materials with Shrinkage of 0.8 - 1 %

Technological properties

Property
Application areas

Air filter housing

Fillers

30% Talc