Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.99 g/cm³

Show Supplier Material materials with Density of 0.99 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural strength

23.0 °C

35 MPa

Show Supplier Material materials with Flexural strength of 35 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

68 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 68 J/m

ASTM D256

Tensile strength

23.0 °C

31 MPa

Show Supplier Material materials with Tensile strength of 31 MPa

ASTM D638

Flexural modulus

ASTM D790

Tear strength

24.0

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

150 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 150 °C

ASTM D648

Melting point

170 °C

Show Supplier Material materials with Melting point of 170 °C

ASTM D2117

Flammability

UL94 V0

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

1 - 1.5 %

Show Supplier Material materials with Shrinkage of 1 - 1.5 %

Technological properties

Property
Application areas

Flame-retardant V0, halogen-free ring, TV parts, electrical parts, holiday lights, Christmas lighting