PP GF50

Alternative and trade names
PP-GF50
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.38 g/cm³

Show Supplier Material materials with Density of 1.38 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

5.1 GPa

Show Supplier Material materials with Flexural modulus of 5.1 GPa

ASTM D790

Flexural strength

23.0 °C

89 MPa

Show Supplier Material materials with Flexural strength of 89 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

195 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 195 J/m

ASTM D256

Tensile strength

23.0 °C

90 MPa

Show Supplier Material materials with Tensile strength of 90 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

160 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C

ASTM D648

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.2 - 0.5 %

Show Supplier Material materials with Shrinkage of 0.2 - 0.5 %

Technological properties

Property
Application areas

High-strength, high-heat-resistant washing machine parts and mechanical parts

Fillers

50% Glass Fiber