PA66 CF40

Alternative and trade names
PA66-CF40
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.33 g/cm³

Show Supplier Material materials with Density of 1.33 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

32 GPa

Show Supplier Material materials with Elastic modulus of 32 GPa

ASTM D790

Elongation

23.0 °C

1 - 2 %

Show Supplier Material materials with Elongation of 1 - 2 %

ASTM D638

Flexural modulus

23.0 °C

28 GPa

Show Supplier Material materials with Flexural modulus of 28 GPa

ASTM D790

Flexural strength

23.0 °C

485 MPa

Show Supplier Material materials with Flexural strength of 485 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

292 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 292 J/m

ASTM D256

Tensile strength

23.0 °C

330 MPa

Show Supplier Material materials with Tensile strength of 330 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

262 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 262 °C

ASTM D648

Melting point

280 °C

Show Supplier Material materials with Melting point of 280 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.2 - 0.3 %

Show Supplier Material materials with Shrinkage of 0.2 - 0.3 %

Technological properties

Property
Application areas

Electrical/electronic applications; industrial components; automotive applications

Fillers

40% Carbon Fiber