Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.1 g/cm³

Show Supplier Material materials with Density of 1.1 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.5 GPa

Show Supplier Material materials with Flexural modulus of 1.5 GPa

ASTM D790

Flexural strength

23.0 °C

60 MPa

Show Supplier Material materials with Flexural strength of 60 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

600 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 600 J/m

ASTM D256

Tensile strength

23.0 °C

50 MPa

Show Supplier Material materials with Tensile strength of 50 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

89 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 89 °C

ASTM D648

Melting point

265 °C

Show Supplier Material materials with Melting point of 265 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

1.4 - 1.8 %

Show Supplier Material materials with Shrinkage of 1.4 - 1.8 %

Technological properties

Property
Application areas

Wheelchair wheels, floor expansion tubes, electrical enclosures, auto parts, rollers, sports equipment, etc.

Fillers

Molybdenum Disulfide