SEBS 7040

Alternative and trade names
TPE 7040
Want to keep this datasheet? Save it now in your required format

Description

TPE-S 40A

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.98 g/cm³

Show Supplier Material materials with Density of 0.98 g/cm³

ASTM D297

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.7 GPa

Show Supplier Material materials with Elastic modulus of 1.7 GPa

Elongation

23.0 °C

900 %

Show Supplier Material materials with Elongation of 900 %

ASTM D412

Hardness, Shore A

23.0 °C

40 [-]

Show Supplier Material materials with Hardness, Shore A of 40 [-]

Tensile strength

23.0 °C

6.5 MPa

Show Supplier Material materials with Tensile strength of 6.5 MPa

ASTM D412

Impact strength, Izod notched, ASTM

No Break

Impact strength, Izod unnotched, ASTM

No Break

Thermal

PropertyValueComment

Max service temperature

100 °C

Show Supplier Material materials with Max service temperature of 100 °C

ASTM D746

Flammability

HB

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1MHz

23.0 °C

2.3 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.3 [-]

ASTM D150

Dielectric strength

23.0 °C

28 kV/mm

Show Supplier Material materials with Dielectric strength of 28 kV/mm

ASTM D149

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

ASTM D150

Volume resistivity

23.0 °C

1.00E+19 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+19 Ω·cm

min., ASTM D257

Technological properties

Property
Application areas

Automotive interior

Fillers

15% Calcium Carbonate

Processing methods

Injection Molding, Extrusion