FR100 series - Halogen free flame retardant Soft PPE

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.1 g/cm³

Show Supplier Material materials with Density of 1.1 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

300 %

Show Supplier Material materials with Elongation of 300 %

ASTM D412

Hardness, Shore A

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Shore A of 90 [-]

ASTM D2240

Tensile strength

23.0 °C

13 MPa

Show Supplier Material materials with Tensile strength of 13 MPa

ASTM D412

Impact strength, Izod notched, ASTM

No Break

Impact strength, Izod unnotched, ASTM

No Break

Thermal

PropertyValue

Flammability

UL 94 V-0

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1MHz

23.0 °C

2.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-]

ASTM D150

Dielectric strength

23.0 °C

28 kV/mm

Show Supplier Material materials with Dielectric strength of 28 kV/mm

ASTM D149

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

ASTM D150

Volume resistivity

23.0 °C

1.00E+19 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+19 Ω·cm

min., ASTM D257

Technological properties

Property
Application areas

Wire & Cable applications

Processing methods

Injection Molding, Extrusion. Pre-drying: 70-80°C for 4-8 Hours, Injection Temperature: 190-240°C, Extrusion Temperature: 180-230°C, Injection pressure: 40-60MPa, Filter: 100-200 mesh