Description

Delene is SEBS based compound, with advantages of soft touch, elasticity, even transparency, Delene is the idea material to replace PVC, natural rubber and silicon rubber in non-fatty contact application.

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Supplier Material materials with Density of 0.9 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compression set

23.0 °C

20 [-]

Show Supplier Material materials with Compression set of 20 [-]

ASTM D395

Elongation

23.0 °C

780 %

Show Supplier Material materials with Elongation of 780 %

ASTM D412

Hardness, Shore A

23.0 °C

10 [-]

Show Supplier Material materials with Hardness, Shore A of 10 [-]

ASTM D2240

Tensile strength

23.0 °C

1.2 MPa

Show Supplier Material materials with Tensile strength of 1.2 MPa

ASTM D412

Thermal

PropertyValueComment

Brittleness temperature

-65 °C

Show Supplier Material materials with Brittleness temperature of -65 °C

D746

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

10 g/10min

Show Supplier Material materials with Melt mass-flow rate of 10 g/10min

D1238, 190°C/5kg

Shrinkage

23.0 °C

2.8 %

Show Supplier Material materials with Shrinkage of 2.8 %

ASTM D955

Technological properties

Property
Processing methods

Extrusion: Hopper Temperature: 130-140°C, Middle Temperature: 140-160°C, Measurment Temperature: 160-180°C, Front Temperature: 170-190°C, Mold Temperature: 160-180°C, Melt Temperature: 150-170°C, Comp. Ratio:3:1, Screen: 20-60 Mesh - Injection:Rear Temperature: 130-140°C, Middle Temperature: 140-160°C, Front Temperature: 160-180°C, Nozzle Temperature: 180-190°C, Melt Temperature:170-180°C, Mold Temperature: 30-80°C, Speed: 100-200rpm, Back Pressure 0.07 - 0.7Mpa