Delon 6055

Alternative and trade names
Delon 6055
Want to keep this datasheet? Save it now in your required format

Description

Delon is a copolymer composed of an aromatic polyester as the hard element and an aliphatic polyether as the soft element. As well as Hytrel TEEE, Delon has excellent heat-aging resistance and oil resistance.

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

450 %

Show Supplier Material materials with Elongation of 450 %

ASTM D412

Flexural strength

23.0 °C

198 MPa

Show Supplier Material materials with Flexural strength of 198 MPa

Hardness, Shore D

23.0 °C

55 [-]

Show Supplier Material materials with Hardness, Shore D of 55 [-]

ASTM D2240

Tear strength

23.0 °C

147 kN/m

Show Supplier Material materials with Tear strength of 147 kN/m

ASTM D624

Tensile strength

23.0 °C

23 MPa

Show Supplier Material materials with Tensile strength of 23 MPa

ASTM D412

Thermal

PropertyValueComment

Brittleness temperature

-70 °C

Show Supplier Material materials with Brittleness temperature of -70 °C

D746

Melting point

200 °C

Show Supplier Material materials with Melting point of 200 °C

Vicat softening temperature

170 °C

Show Supplier Material materials with Vicat softening temperature of 170 °C

Technological properties

Property
Processing methods

Pre-drying: 100°C for 4-8 hr, Injection temperature: 10-20°C higher than melting temperature, Extrusion and blow temperature: higher than melting temperature