TPE Delene 5590

Alternative and trade names
Delene 5590
Want to keep this datasheet? Save it now in your required format

Description

Halogen free flame retardant TPE for Wire & Cable applications, with excellent elasticity

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

450 %

Show Supplier Material materials with Elongation of 450 %

ASTM D412

Hardness, Shore A

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Shore A of 90 [-]

ASTM D2240

Hardness, Shore D

23.0 °C

35 [-]

Show Supplier Material materials with Hardness, Shore D of 35 [-]

ASTM D2240

Tensile strength

23.0 °C

10 MPa

Show Supplier Material materials with Tensile strength of 10 MPa

ASTM D412

Thermal

PropertyValue

Flammability

UL94 V-0 (3mm)

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

min., ASTM D149

Volume resistivity

23.0 °C

1.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm

min., ASTM D257

Technological properties

Property
Application areas

Wire & Cable applications

Processing methods

Hopper Temperature: 150-170°C, Transmission Temperature: 180-200°C, Measurement Temperature: 200-230°C, Die Temperature: 190-220°C