Description

High tensile strength, excellent elongation, and fatigue resistance enable optimized design and light weighting.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.76 g/cm³

Show Material materials with Density of 2.76 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

70 - 72 GPa

Show Material materials with Elastic modulus of 70 - 72 GPa

Elongation

23.0 °C

8 - 12 %

Show Material materials with Elongation of 8 - 12 %

Fatigue strength

23.0 °C

100 MPa

Show Material materials with Fatigue strength of 100 MPa

measured after 10⁷ cycles, R = 1

Tensile strength

23.0 °C

375 - 400 MPa

Show Material materials with Tensile strength of 375 - 400 MPa

Yield strength

23.0 °C

320 - 350 MPa

Show Material materials with Yield strength of 320 - 350 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.19E-5 - 2.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.19E-5 - 2.9E-5 1/K

measured from 20-300°C

Melting point

475 - 642 °C

Show Material materials with Melting point of 475 - 642 °C

Thermal conductivity

23.0 °C

152 - 200 W/(m·K)

Show Material materials with Thermal conductivity of 152 - 200 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

2.09E+7 - 2.49E+7 S/m

Show Material materials with Electrical conductivity of 2.09E+7 - 2.49E+7 S/m

Chemical properties

PropertyValue

Aluminium

balance

Copper

0.35 - 1 %

Show Material materials with Copper of 0.35 - 1 %

Iron

0 - 0.15 %

Show Material materials with Iron of 0 - 0.15 %

Magnesium

1 - 2 %

Show Material materials with Magnesium of 1 - 2 %

Manganese

0 - 0.1 %

Show Material materials with Manganese of 0 - 0.1 %

Other

0 - 0.15 %

Show Material materials with Other of 0 - 0.15 %

Silicon

0 - 0.15 %

Show Material materials with Silicon of 0 - 0.15 %

Titanium

0 - 0.2 %

Show Material materials with Titanium of 0 - 0.2 %

Vanadium

0.05 - 0.3 %

Show Material materials with Vanadium of 0.05 - 0.3 %

Zinc

4 - 5.5 %

Show Material materials with Zinc of 4 - 5.5 %

Zirconium

0.05 - 0.3 %

Show Material materials with Zirconium of 0.05 - 0.3 %

Technological properties

Property
Application areas

Suspension components, steering knuckles, control arms

Corrosion properties

Good SCC and general corrosion resistance

General machinability

Very good machinability

Processing history

Temper: T6

Processing methods

Melt treatment and casting: Grain refinement with Ti-B is required, addition of Ti-B improves castability, casting temperature: 680°C to 720°C