General
Property | Value |
---|---|
Density | 0.91 - 1.5 g/cm³ Show Material materials with Density of 0.91 - 1.5 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 100.0 - 800.0 % Show Material materials with Elongation of 100.0 - 800.0 % | |
Tensile strength | 4.0 - 30.0 MPa Show Material materials with Tensile strength of 4.0 - 30.0 MPa | at 100-800% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.000180 1/K Show Material materials with Coefficient of thermal expansion of 0.000180 1/K |
Specific heat capacity | 1900.0 - 2000.0 J/(kg·K) Show Material materials with Specific heat capacity of 1900.0 - 2000.0 J/(kg·K) |
Thermal conductivity | 0.17 - 0.25 W/(m·K) Show Material materials with Thermal conductivity of 0.17 - 0.25 W/(m·K) |
Flammability | UL 94 HB |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Tires, cable sheathing, hoses, profiles, foam rubber | |
Processing methods | Compression molding, extrusion, vulcanization |