Styrene butadiene rubber (SBR)

Alternative and trade names
Sprintan™, Buna®, Europrene®
Want to keep this datasheet? Save it now in your required format

Description

Styrene butadiene rubber (SBR) has a good abrasion resistance and good aging stability when protected by additives.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

0.91 - 1.5 g/cm³

Show Material materials with Density of 0.91 - 1.5 g/cm³

Mechanical

PropertyValueComment

Elongation

100.0 - 800.0 %

Show Material materials with Elongation of 100.0 - 800.0 %

Tensile strength

4.0 - 30.0 MPa

Show Material materials with Tensile strength of 4.0 - 30.0 MPa

at 100-800% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.000180 1/K

Show Material materials with Coefficient of thermal expansion of 0.000180 1/K

Specific heat capacity

1900.0 - 2000.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1900.0 - 2000.0 J/(kg·K)

Thermal conductivity

0.17 - 0.25 W/(m·K)

Show Material materials with Thermal conductivity of 0.17 - 0.25 W/(m·K)

Flammability

UL 94 HB

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Tires, cable sheathing, hoses, profiles, foam rubber

Processing methods

Compression molding, extrusion, vulcanization