SMP monocrystalline synthetic SmartMicron diamond powder, standard size range

Want to keep this datasheet? Save it now in your required format

Description

SMP SmartMicron diamond powder is made of modified synthetic diamond. SmartMicron diamond products deliver outstanding performance in lapping processes of superhard materials such as sapphire, ceramics and hard metals. Compared to conventional diamond powders, SmartMicron diamond powder delivers typically 10–20 % higher material removal rates (MRR) at equivalent values of surface roughness.


Best performance: For best performance, we recommend to use SmartMicron products incorporated in our state-of-the-art diamond suspension formulations. The product range includes oil based and water soluble suspension formulations.

This material data has been provided by Pureon.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

3.51 g/cm³

Show Supplier Material materials with Density of 3.51 g/cm³

Particle size range

2 - 8 µm

Show Supplier Material materials with Particle size range of 2 - 8 µm

Please refer to the technological properties section below for more detailed (narrow) particle size ranges available.

Mechanical

PropertyValue

Hardness, Mohs

10 [-]

Show Supplier Material materials with Hardness, Mohs of 10 [-]

Thermal

PropertyValue

Coefficient of thermal expansion

1.1e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.1e-06 1/K

Thermal conductivity

600 - 4000 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 600 - 4000 W/(m·K)

Electrical

PropertyValue

Band gap

6 eV

Show Supplier Material materials with Band gap of 6 eV

Electrical resistivity

1e+12 - 1e+19 Ω·m

Show Supplier Material materials with Electrical resistivity of 1e+12 - 1e+19 Ω·m

Optical

PropertyValue

Refractive index

2 [-]

Show Supplier Material materials with Refractive index of 2 [-]

Chemical properties

PropertyValueComment

Carbon

99 %

Show Supplier Material materials with Carbon of 99 %

min. purity

Technological properties

Property
Application areas

SMP SmartMicron diamond powder is ideal for lapping applications requiring a high stock removal. Typical applications include lapping of sapphire, ceramics, tungsten carbide and hard metals.

Color

Yellowish

Crystal structure

Monocrystalline

Gradings

Standard size range: The standard size range makes this product suitable for applications with a focus on economics. The controlled upper limit ensures a uniform, scratch-free surface quality.

Morphology

Structured particle surface: The micro-structured, rough particle surface maximizes the material removal rate due to the numerous contact points provided between diamond particles and the work piece.

Particle size range table

Micron Size
µm
Median (D50)
µm
Median-Tolerance
µm
Upper Limit (D99)
µm max.
SMP3   (2-4)3.12.82-3.385
SMP4   (2-6)4.23.82-4.586.7
SMP5   (3-7)5.34.82-5.788
SMP6   (4-8)6.35.73-6.879.5

Synthesis