The material: 'DIN 1725-1 Grade AlMgSi0.5' you were looking for has been superseded by the one below.

DIN 1725-1 Grade 3.2305

Want to keep this datasheet? Save it now in your required format

Description

E-AlMgSi is ensured by the German electrotechnical commission as electrical conductive material according to DIN 40 501 part of 1 to part of 4. This cold and warm formable material reaches mechanical strength from 200 to 250 MPa with A5-elongations at break of approx. 10 %. In warm and cold hardened state this alloy is only limited formable, in the soft material condition however well. Weldability, corrosion resistance and anodising ability of this material are good. The alloy E-AlMgSi is ensured by a purposeful heat treatment apart from the strength increase an appropriate high electrical conductivity, so that it is applicable for statically loaded elements in electro-technology. heat treatment for hardening: solution annealing: 525 to 540 °C, quenching in water cold ageing: 5 to 8 d on ambient temperature warm ageing: 4 to 16 h at 155 to 190 °C Application: Electro-technology (overhead line)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueRelated Standards

Density

20.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

DIN 1725-1, EN 573-3, EN 573-4

Mechanical

PropertyTemperatureValueRelated StandardsComment

Elastic modulus

20.0 °C

68.0 GPa

Show Material materials with Elastic modulus of 68.0 GPa

DIN 1725-1, EN 573-3, EN 573-4

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

20.0 °C

26.5 - 27.0 GPa

Show Material materials with Shear modulus of 26.5 - 27.0 GPa

DIN 1725-1, EN 573-3, EN 573-4

Thermal

PropertyTemperatureValueRelated StandardsComment

Coefficient of thermal expansion

1.6e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 6000 Series Aluminium

Melting point

555.0 - 655.0 °C

Show Material materials with Melting point of 555.0 - 655.0 °C

Typical for Wrought 6000 Series Aluminium

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

20.0 °C

210.0 W/(m·K)

Show Material materials with Thermal conductivity of 210.0 W/(m·K)

DIN 1725-1, EN 573-3, EN 573-4

Electrical

PropertyValueComment

Electrical conductivity

21000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 - 34000000.0 S/m

Typical for Wrought 6000 Series Aluminium

Electrical resistivity

2.9e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5e-08 Ω·m

Typical for Wrought 6000 Series Aluminium

Chemical properties

PropertyValueRelated Standards

Copper

0.02

Show Material materials with Copper of 0.02

DIN 1725-1, EN 573-3, EN 573-4

Iron

0.1 - 0.3 %

Show Material materials with Iron of 0.1 - 0.3 %

DIN 1725-1, EN 573-3, EN 573-4

Magnesium

0.35 - 0.6 %

Show Material materials with Magnesium of 0.35 - 0.6 %

DIN 1725-1, EN 573-3, EN 573-4

Silicon

0.5 - 0.6 %

Show Material materials with Silicon of 0.5 - 0.6 %

DIN 1725-1, EN 573-3, EN 573-4

Zinc

0.15

Show Material materials with Zinc of 0.15

DIN 1725-1, EN 573-3, EN 573-4

Technological properties

Property
Workability

Excellent workability.