Master alloy produced by melting. Color code: red

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueRelated Standards

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

EN 575, DIN 1725-3

Copper

0.2 %

Show Material materials with Copper of 0.2 %

EN 575, DIN 1725-3

Iron

0.7 %

Show Material materials with Iron of 0.7 %

EN 575, DIN 1725-3

0.70 %

Show Material materials with Iron of 0.70 %

EN 575

Magnesium

0.5 %

Show Material materials with Magnesium of 0.5 %

EN 575, DIN 1725-3

Manganese

0.4 %

Show Material materials with Manganese of 0.4 %

EN 575, DIN 1725-3

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

EN 575, DIN 1725-3

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

EN 575, DIN 1725-3

Titanium

4.5 - 5.5 %

Show Material materials with Titanium of 4.5 - 5.5 %

EN 575, DIN 1725-3

Vanadium

0.3 %

Show Material materials with Vanadium of 0.3 %

EN 575, DIN 1725-3

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %