General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 2.65 - 2.7 g/cm³ Show Material materials with Density of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 73 - 80 GPa Show Material materials with Elastic modulus of 73 - 80 GPa | Typical for Cast 3xx.x Series Aluminium |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Shear modulus | 23.0 °C | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 2.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 2.3E-5 1/K | Typical for Cast 3xx.x Series Aluminium |
Melting point | 505 - 770 °C Show Material materials with Melting point of 505 - 770 °C | Typical for Cast 3xx.x Series Aluminium | |
Specific heat capacity | 23.0 °C | 960 - 963 J/(kg·K) Show Material materials with Specific heat capacity of 960 - 963 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Thermal conductivity | 23.0 °C | 130 - 180 W/(m·K) Show Material materials with Thermal conductivity of 130 - 180 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 82.9999 - 90.4999 % Show Material materials with Aluminium of 82.9999 - 90.4999 % |
Copper | 2 - 4 % Show Material materials with Copper of 2 - 4 % |
Iron | 0.9 % Show Material materials with Iron of 0.9 % |
Magnesium | 0.3 % Show Material materials with Magnesium of 0.3 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silicon | 7.5 - 9.5 % Show Material materials with Silicon of 7.5 - 9.5 % |
Tin | 0.3 % Show Material materials with Tin of 0.3 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |