General
Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.71 g/cm³ Show Material materials with Density of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 71.0 - 75.0 GPa Show Material materials with Elastic modulus of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2e-05 - 2.2e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Melting point | 565.0 - 630.0 °C Show Material materials with Melting point of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Thermal conductivity | 130.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | JIS H5202 |
Copper | 0.5 - 1.5 % Show Material materials with Copper of 0.5 - 1.5 % | JIS H5202 |
Iron | 0.80 % Show Material materials with Iron of 0.80 % | JIS H5202 |
Lead | 0.1 % Show Material materials with Lead of 0.1 % | JIS H5202 |
Magnesium | 0.5 - 1.5 % Show Material materials with Magnesium of 0.5 - 1.5 % | JIS H5202 |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % | JIS H5202 |
Nickel | 0.5 - 1.5 % Show Material materials with Nickel of 0.5 - 1.5 % | JIS H5202 |
Silicon | 18.0 - 20.0 % Show Material materials with Silicon of 18.0 - 20.0 % | JIS H5202 |
Tin | 0.1 % Show Material materials with Tin of 0.1 % | JIS H5202 |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % | JIS H5202 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | JIS H5202 |