General
Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.71 g/cm³ Show Material materials with Density of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 71.0 - 75.0 GPa Show Material materials with Elastic modulus of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | ||
Elongation | 3.5 % Show Material materials with Elongation of 3.5 % | ASTM B85 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | ||
Shear strength | 170.0 MPa Show Material materials with Shear strength of 170.0 MPa | ASTM B85 | Casting | |
Tensile strength | 290.0 MPa Show Material materials with Tensile strength of 290.0 MPa | ASTM B85 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2e-05 - 2.2e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Melting point | 565.0 - 630.0 °C Show Material materials with Melting point of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Thermal conductivity | 130.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 1.0 Show Material materials with Copper of 1.0 | ASTM B85 | Casting |
Iron | 1.3 Show Material materials with Iron of 1.3 | ASTM B85 | Casting |
Magnesium | 0.1 Show Material materials with Magnesium of 0.1 | ASTM B85 | Casting |
Manganese | 0.35 Show Material materials with Manganese of 0.35 | ASTM B85 | Casting |
Nickel | 0.5 Show Material materials with Nickel of 0.5 | ASTM B85 | Casting |
Silicon | 11.0 - 13.0 % Show Material materials with Silicon of 11.0 - 13.0 % | ASTM B85 | Casting |
Tin | 0.15 Show Material materials with Tin of 0.15 | ASTM B85 | Casting |
Zinc | 0.5 Show Material materials with Zinc of 0.5 | ASTM B85 | Casting |
Do you have a technical question or need more information about this material?