"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.6 - 2.7 g/cm³

Show Material materials with Density of 2.6 - 2.7 g/cm³

Typical for Cast 5xx.x Series Aluminium

Mechanical

PropertyValueRelated StandardsShapeComment

Elastic modulus

68.0 - 70.0 GPa

Show Material materials with Elastic modulus of 68.0 - 70.0 GPa

Typical for Cast 5xx.x Series Aluminium

Elongation

4.0 %

Show Material materials with Elongation of 4.0 %

ASTM B85

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 5xx.x Series Aluminium

Shear strength

200.0 MPa

Show Material materials with Shear strength of 200.0 MPa

ASTM B85

Casting

Tensile strength

310.0 MPa

Show Material materials with Tensile strength of 310.0 MPa

ASTM B85

Casting

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.3e-05 - 2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3e-05 - 2.5e-05 1/K

Typical for Cast 5xx.x Series Aluminium

Melting point

450.0 - 640.0 °C

Show Material materials with Melting point of 450.0 - 640.0 °C

Typical for Cast 5xx.x Series Aluminium

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 5xx.x Series Aluminium

Thermal conductivity

60.0 - 140.0 W/(m·K)

Show Material materials with Thermal conductivity of 60.0 - 140.0 W/(m·K)

Typical for Cast 5xx.x Series Aluminium

Chemical properties

PropertyValueRelated StandardsShape

Copper

0.25

Show Material materials with Copper of 0.25

ASTM B85

Casting

Iron

1.8

Show Material materials with Iron of 1.8

ASTM B85

Casting

Magnesium

7.5 - 8.5 %

Show Material materials with Magnesium of 7.5 - 8.5 %

ASTM B85

Casting

Manganese

0.35

Show Material materials with Manganese of 0.35

ASTM B85

Casting

Nickel

0.15

Show Material materials with Nickel of 0.15

ASTM B85

Casting

Silicon

0.35

Show Material materials with Silicon of 0.35

ASTM B85

Casting

Tin

0.15

Show Material materials with Tin of 0.15

ASTM B85

Casting

Zinc

0.15

Show Material materials with Zinc of 0.15