General
Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.7 g/cm³ Show Material materials with Density of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 73.0 - 80.0 GPa Show Material materials with Elastic modulus of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Elongation | 2.5 % Show Material materials with Elongation of 2.5 % | ASTM B85 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Shear modulus | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Shear strength | 190.0 MPa Show Material materials with Shear strength of 190.0 MPa | ASTM B85 | Casting | |
Tensile strength | 315.0 MPa Show Material materials with Tensile strength of 315.0 MPa | ASTM B85 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Melting point | 505.0 - 770.0 °C Show Material materials with Melting point of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Specific heat capacity | 960.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Thermal conductivity | 130.0 - 180.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 3.0 - 4.0 % Show Material materials with Copper of 3.0 - 4.0 % | ASTM B85 | Casting |
Iron | 2.0 Show Material materials with Iron of 2.0 | ASTM B85 | Casting |
Magnesium | 0.1 Show Material materials with Magnesium of 0.1 | ASTM B85 | Casting |
Manganese | 0.5 Show Material materials with Manganese of 0.5 | ASTM B85 | Casting |
Nickel | 0.5 Show Material materials with Nickel of 0.5 | ASTM B85 | Casting |
Silicon | 7.5 - 9.5 % Show Material materials with Silicon of 7.5 - 9.5 % | ASTM B85 | Casting |
Tin | 0.35 Show Material materials with Tin of 0.35 | ASTM B85 | Casting |
Zinc | 3.0 Show Material materials with Zinc of 3.0 | ASTM B85 | Casting |