General
Property | Value | Comment |
---|---|---|
Density | 2.6 - 2.7 g/cm³ Show Material materials with Density of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Elongation | 7.0 % Show Material materials with Elongation of 7.0 % | F | ASTM B108 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Tensile strength | 240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | F | ASTM B108 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Melting point | 450.0 - 640.0 °C Show Material materials with Melting point of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Thermal conductivity | 60.0 - 140.0 W/(m·K) Show Material materials with Thermal conductivity of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Beryllium | 0.003 - 0.007 % Show Material materials with Beryllium of 0.003 - 0.007 % | F | ASTM B108 | Casting |
Boron | 0.005 Show Material materials with Boron of 0.005 | F | ASTM B108 | Casting |
Copper | 0.05 Show Material materials with Copper of 0.05 | F | ASTM B108 | Casting |
Iron | 0.15 Show Material materials with Iron of 0.15 | F | ASTM B108 | Casting |
Magnesium | 6.2 - 7.5 % Show Material materials with Magnesium of 6.2 - 7.5 % | F | ASTM B108 | Casting |
Manganese | 0.1 - 0.25 % Show Material materials with Manganese of 0.1 - 0.25 % | F | ASTM B108 | Casting |
Silicon | 0.15 Show Material materials with Silicon of 0.15 | F | ASTM B108 | Casting |
Titanium | 0.1 - 0.25 % Show Material materials with Titanium of 0.1 - 0.25 % | F | ASTM B108 | Casting |