General
Property | Value | Comment |
---|---|---|
Density | 2.8 g/cm³ Show Material materials with Density of 2.8 g/cm³ | Typical for Cast 8xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | Typical for Cast 8xx.x Series Aluminium | |||
Elongation | 3.0 % Show Material materials with Elongation of 3.0 % | T5 | ASTM B108 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 8xx.x Series Aluminium | |||
Tensile strength | 115.0 MPa Show Material materials with Tensile strength of 115.0 MPa | T5 | ASTM B108 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K | Typical for Cast 8xx.x Series Aluminium |
Melting point | 205.0 - 650.0 °C Show Material materials with Melting point of 205.0 - 650.0 °C | Typical for Cast 8xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 8xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 0.7 - 1.3 % Show Material materials with Copper of 0.7 - 1.3 % | T5 | ASTM B108 | Casting |
Iron | 0.7 Show Material materials with Iron of 0.7 | T5 | ASTM B108 | Casting |
Magnesium | 0.1 Show Material materials with Magnesium of 0.1 | T5 | ASTM B108 | Casting |
Manganese | 0.1 Show Material materials with Manganese of 0.1 | T5 | ASTM B108 | Casting |
Nickel | 0.3 - 0.7 % Show Material materials with Nickel of 0.3 - 0.7 % | T5 | ASTM B108 | Casting |
Silicon | 2.0 - 3.0 % Show Material materials with Silicon of 2.0 - 3.0 % | T5 | ASTM B108 | Casting |
Tin | 5.5 - 7.0 % Show Material materials with Tin of 5.5 - 7.0 % | T5 | ASTM B108 | Casting |
Titanium | 0.2 Show Material materials with Titanium of 0.2 | T5 | ASTM B108 | Casting |