AA 206.0 T6

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

3.0 g/cm³

Show Material materials with Density of 3.0 g/cm³

T6

Mechanical

PropertyValueConditionComment

Charpy impact energy, V-notch

5.0 - 15.0 J

Show Material materials with Charpy impact energy, V-notch of 5.0 - 15.0 J

T6

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

T6

71 GPa

Show Material materials with Elastic modulus of 71 GPa

T6

Elongation

9.0 %

Show Material materials with Elongation of 9.0 %

T6

6.0 - 12.0 %

Show Material materials with Elongation of 6.0 - 12.0 %

T6

Sand cast, elongation in 50 mm

Hardness, Brinell

135 [-]

Show Material materials with Hardness, Brinell of 135 [-]

T6

500 kg load, 10 mm b

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

T6

Shear modulus

23.0 GPa

Show Material materials with Shear modulus of 23.0 GPa

T6

Shear strength

255 MPa

Show Material materials with Shear strength of 255 MPa

T6

Tensile strength

390.0 MPa

Show Material materials with Tensile strength of 390.0 MPa

T6

345.0 - 380.0 MPa

Show Material materials with Tensile strength of 345.0 - 380.0 MPa

T6

Sand cast

Yield strength

240.0 MPa

Show Material materials with Yield strength of 240.0 MPa

T6

205.0 - 240.0 MPa

Show Material materials with Yield strength of 205.0 - 240.0 MPa

T6

Sand cast, RP02

Thermal

PropertyValueCondition

Coefficient of thermal expansion

2.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K

T6

Melting point

570.0 °C

Show Material materials with Melting point of 570.0 °C

T6

Specific heat capacity

920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 920.0 J/(kg·K)

T6

Thermal conductivity

120.0 W/(m·K)

Show Material materials with Thermal conductivity of 120.0 W/(m·K)

T6

Electrical

PropertyValueComment

Electrical conductivity

16000000.0 - 23000000.0 S/m

Show Material materials with Electrical conductivity of 16000000.0 - 23000000.0 S/m

Typical for Cast 2xx.x Series Aluminium

Electrical resistivity

4.347826086956522e-08 - 6.25e-08 Ω·m

Show Material materials with Electrical resistivity of 4.347826086956522e-08 - 6.25e-08 Ω·m

Typical for Cast 2xx.x Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

93.3 - 95.3 %

Show Material materials with Aluminium of 93.3 - 95.3 %

T6

Copper

4.2 - 5.0 %

Show Material materials with Copper of 4.2 - 5.0 %

T6

Iron

0.15 %

Show Material materials with Iron of 0.15 %

T6

Magnesium

0.15 - 0.35 %

Show Material materials with Magnesium of 0.15 - 0.35 %

T6

Manganese

0.2 - 0.5 %

Show Material materials with Manganese of 0.2 - 0.5 %

T6

Nickel

0.05 %

Show Material materials with Nickel of 0.05 %

T6

Other

0.15 %

Show Material materials with Other of 0.15 %

T6

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

T6

Tin

0.05 %

Show Material materials with Tin of 0.05 %

T6

Titanium

0.15 - 0.3 %

Show Material materials with Titanium of 0.15 - 0.3 %

T6

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

T6