See where AA 206.0 T7 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ3 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.1E-5 1/K at 23 °C
Melting point
Tm570 °C
Specific heat capacity
cp920 J/(kg·K) at 23 °C
Thermal conductivity
λ120 W/(m·K) at 23 °C
Electrical conductivity
σel1.60E+7 - 2.30E+7 S/m at 23 °C
Typical for Cast 2xx.x Series Aluminium
Electrical resistivity
ρel5E-8 - 5.4E-8 Ω·m at 23 °C
Typical values
Element
Weight %
Comment
93.3 - 95.3 %
4.2 - 5 %
0.2 - 0.5 %
0.15 - 0.35 %
0.15 - 0.3 %
This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials.