General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 3 g/cm³ Show Material materials with Density of 3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 78 GPa Show Material materials with Elastic modulus of 78 GPa |
Elongation | 20.0 °C | 2.1 % Show Material materials with Elongation of 2.1 % |
Tensile strength | 20.0 °C | 150 MPa Show Material materials with Tensile strength of 150 MPa |
Yield strength | 20.0 °C | 110 MPa Show Material materials with Yield strength of 110 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Melting point | 540 °C Show Material materials with Melting point of 540 °C | |
Specific heat capacity | 20.0 °C | 860 J/(kg·K) Show Material materials with Specific heat capacity of 860 J/(kg·K) |
Thermal conductivity | 20.0 °C | 110 W/(m·K) Show Material materials with Thermal conductivity of 110 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 85.8 - 91.5 % Show Material materials with Aluminium of 85.8 - 91.5 % |
Copper | 3 - 4 % Show Material materials with Copper of 3 - 4 % |
Iron | 1 % Show Material materials with Iron of 1 % |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 0.35 % Show Material materials with Nickel of 0.35 % |
Other | 0.5 % Show Material materials with Other of 0.5 % |
Silicon | 5.5 - 6.5 % Show Material materials with Silicon of 5.5 - 6.5 % |
Titanium | 0.25 % Show Material materials with Titanium of 0.25 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |