355.0-T6 Aluminium

.XLSX
.PDF
Save

Properties

Electrical

Electrical conductivity σel

2.20E+8 S/m at 20 °C

General

Density ρ

2.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

76 GPa at 20 °C

Elongation A

2.6 % at 20 °C

Tensile strength Rm

260 MPa at 20 °C

Yield strength YS

170 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.3E-5 1/K at 20 °C

Melting point Tm

560 °C

Specific heat capacity cp

880 J/(kg·K) at 20 °C

Thermal conductivity λ

150 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

90.3 - 94.1 %

Si

4.5 - 5.5 %

Cu

1 - 1.5 %

Mg

0.4 - 0.6 %

Zn

0 - 0.35 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.