See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 23 °C
Elongation
ASand cast, elongation in 50 mm
Coefficient of thermal expansion
α2.2E-5 1/K at 23 °C
Melting point
Tm557 - 613 °C
Specific heat capacity
cp970 J/(kg·K) at 23 °C
derived value
Thermal conductivity
λ150 W/(m·K) at 23 °C
derived value
Electrical conductivity
σel2.30E+7 S/m at 23 °C
Typical/Derived values
Electrical resistivity
ρel4.42E-8 Ω·m at 23 °C
Typical values
Specific Electrical conductivity
39 - 41 % IACS
Typical values
Element
Weight %
Comment
90.1 - 93.3 %
6.5 - 7.5 %
0.2 - 0.45 %
0 - 0.25 %
0 - 0.6 %
This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials,CastAl_Thermal,AluKey.