Pink Sheets Grade 356.0 T71

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

T71

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

72.0 GPa

Show Material materials with Elastic modulus of 72.0 GPa

T71

72.4 GPa

Show Material materials with Elastic modulus of 72.4 GPa

T71

Elongation

3.0 %

Show Material materials with Elongation of 3.0 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

A100

3.5 %

Show Material materials with Elongation of 3.5 %

T71

3.5 %

Show Material materials with Elongation of 3.5 %

T71

Sand cast, elongation in 50 mm

Fatigue strength

59 MPa

Show Material materials with Fatigue strength of 59 MPa

T71

for 5x10⁸ cycles, R.R. Moore type test

Hardness, Brinell

60 [-]

Show Material materials with Hardness, Brinell of 60 [-]

T71

500 kg load, 10 mm b

60.0 [-]

Show Material materials with Hardness, Brinell of 60.0 [-]

T71

Pink Sheets, ASTM B618

Casting

70.0 [-]

Show Material materials with Hardness, Brinell of 70.0 [-]

T71

Pink Sheets, ASTM B108

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

T71

Shear modulus

27.2 GPa

Show Material materials with Shear modulus of 27.2 GPa

T71

Shear strength

138 MPa

Show Material materials with Shear strength of 138 MPa

T71

Tensile strength

150.0 MPa

Show Material materials with Tensile strength of 150.0 MPa

T71

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

193 MPa

Show Material materials with Tensile strength of 193 MPa

T71

Sand cast

Yield strength

125.0 MPa

Show Material materials with Yield strength of 125.0 MPa

T71

Pink Sheets, ASTM B618

Casting

RP02

140.0 MPa

Show Material materials with Yield strength of 140.0 MPa

T71

145 MPa

Show Material materials with Yield strength of 145 MPa

T71

Sand cast, RP02

Thermal

PropertyValueConditionRelated StandardsShape

Coefficient of thermal expansion

2.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 1/K

T71

Melting point

557.0 - 613.0 °C

Show Material materials with Melting point of 557.0 - 613.0 °C

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

570.0 °C

Show Material materials with Melting point of 570.0 °C

T71

Specific heat capacity

970.0 J/(kg·K)

Show Material materials with Specific heat capacity of 970.0 J/(kg·K)

T71

Thermal conductivity

160.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 W/(m·K)

T71

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

90.1 - 93.3 %

Show Material materials with Aluminium of 90.1 - 93.3 %

T71

Copper

0.25 %

Show Material materials with Copper of 0.25 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Iron

0.6 %

Show Material materials with Iron of 0.6 %

T71

0.60 %

Show Material materials with Iron of 0.60 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Magnesium

0.2 - 0.45 %

Show Material materials with Magnesium of 0.2 - 0.45 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Manganese

0.35 %

Show Material materials with Manganese of 0.35 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Other

0.15 %

Show Material materials with Other of 0.15 %

T71

Silicon

6.5 - 7.5 %

Show Material materials with Silicon of 6.5 - 7.5 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Titanium

0.25 %

Show Material materials with Titanium of 0.25 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting

Zinc

0.35 %

Show Material materials with Zinc of 0.35 %

T71

Pink Sheets, ASTM B108, ASTM B618

Casting