See where AA A360.0 O falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.2E-5 1/K at 23 °C
Melting point
Tm590 °C
Specific heat capacity
cp960 J/(kg·K) at 23 °C
Thermal conductivity
λ110 W/(m·K) at 23 °C
Element
Weight %
Comment
85.8 - 90.6 %
9 - 10 %
0.4 - 0.6 %
0 - 0.6 %
0 - 1.3 %