Description

Nanoker produces ceramic components and tailor made products from KA997. The key benefits of Aluminum Oxide 99.78% (KA997) are: Low coefficient of friction, excellent wear resistance, high corrosion resistance, good thermal conductivity, good dielectric properties.

This material data has been provided by Nanoker.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

3.9 g/cm³

Show Supplier Material materials with Density of 3.9 g/cm³

Porosity

0 %

Show Supplier Material materials with Porosity of 0 %

open porositiy

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

370 GPa

Show Supplier Material materials with Elastic modulus of 370 GPa

Flexural strength

23.0 °C

400 MPa

Show Supplier Material materials with Flexural strength of 400 MPa

Plane-Strain Fracture Toughnes

23.0 °C

3.5 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.5 MPa·√m

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

1000.0 °C

8.6E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8.6E-6 1/K

Max service temperature

1550 °C

Show Supplier Material materials with Max service temperature of 1550 °C

no load

Thermal conductivity

23.0 °C

28 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 28 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.00E+11 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+11 Ω·m

Chemical properties

PropertyValueComment

Aluminium

99.78 %

Show Supplier Material materials with Aluminium of 99.78 %

as Al₂O₃

Calcium

0.05 %

Show Supplier Material materials with Calcium of 0.05 %

as CaO

Iron

0.03 %

Show Supplier Material materials with Iron of 0.03 %

as Fe₂O₃

Magnesium

0.1 %

Show Supplier Material materials with Magnesium of 0.1 %

as MgO

Silicon

0.05 %

Show Supplier Material materials with Silicon of 0.05 %

as SiO₂

Technological properties

Property
Application areas

Typical application areas include: High temperature labware, furnace construction, abrasives industry, mechanical engineering, pump & compressor industry, chemical & pharmaceutical industry