Nanoker produces ceramic components and tailor made products from KFSZ. The key benefits of Fully Stabilized Zirconia (KFSZ) are: High purity and density, good corrosion resistance. high oxygen conductivity, high temperature resistance.
See where Fully Stabilized Zirconia (KFSZ) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ5.7 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.1E-5 1/K at 1000 °C
Max service temperature
Tmax2000 °C
no load
Thermal conductivity
λ2.5 W/(m·K) at 23 °C
Electrical resistivity
ρel1.00E+13 Ω·m at 23 °C
Element
Weight %
Comment
99.7 %
as ZrO₂ + HfO₂ + Y₂O₃
13.3 %
as Y₂O₃
0.02 %
as SiO₂
0.01 %
as Fe₂O₃
5E-3 %
as Na₂O
Application areas
Typical application areas include: Oxygen sensors and solid oxide fuel cells (SOFC)
This material data has been provided by Nanoker.