Description

Chloroprene latex impregnated E glass cord (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

300 N

Show Supplier Material materials with Adhesion of 300 N

min., Cold U Test

Linear density

23.0 °C

0.06 - 0.07 g/cm

Show Supplier Material materials with Linear density of 0.06 - 0.07 g/cm

Dimension

PropertyValueComment

Bobbin Inner Diameter

57 - 63 mm

Show Supplier Material materials with Bobbin Inner Diameter of 57 - 63 mm

tapered

Bobbin Length

341 mm

Show Supplier Material materials with Bobbin Length of 341 mm

Diameter

2.5 - 2.9 mm

Show Supplier Material materials with Diameter of 2.5 - 2.9 mm

Apparent Diameter

Flange Diameter

279.5 mm

Show Supplier Material materials with Flange Diameter of 279.5 mm

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2.3 - 3.7 %

Show Supplier Material materials with Elongation of 2.3 - 3.7 %

Nominal breaking force

23.0 °C

2500 N

Show Supplier Material materials with Nominal breaking force of 2500 N

Tensile Member: E Glass

Technological properties

Property
Color

Black

Cord Construction

330.3/5

Other

Manufacturing Location: Canada

Processing history

Latex Type: Chloroprene, Dip Pick-Up: 19 to 28%

Twist per Meter

32 - 46 TPM

Direction: S & Z