Glass cord G10-060128 / G10-060228

Alternative and trade names
Glass Cord
Want to keep this datasheet? Save it now in your required format

Description

NBR latex impregnated carbon fibre cord (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

125 N

Show Supplier Material materials with Adhesion of 125 N

min., Hot U Test

Linear density

23.0 °C

0.01 g/cm

Show Supplier Material materials with Linear density of 0.01 g/cm

Dimension

PropertyValue

Bobbin Inner Diameter

60 mm

Show Supplier Material materials with Bobbin Inner Diameter of 60 mm

Bobbin Length

356 mm

Show Supplier Material materials with Bobbin Length of 356 mm

Flange Diameter

159 mm

Show Supplier Material materials with Flange Diameter of 159 mm

Mechanical

PropertyTemperatureValueComment

Nominal breaking force

23.0 °C

800 N

Show Supplier Material materials with Nominal breaking force of 800 N

Tensile Member: Carbon Fibre

Technological properties

Property
Color

Black

Cord Construction

800.1/0

Other

Manufacturing Location: Canada

Processing history

Latex Type: NBR, Dip Pick-Up: 20 to 30%

Twist per Meter

52 - 68 TPM

Direction: S & Z