Chopped Strand H33-006002

Alternative and trade names
Glass Strand
Want to keep this datasheet? Save it now in your required format

Description

SBR latex impregnated E glass chopped strand (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValueComment

Length

3 - 9 mm

Show Supplier Material materials with Length of 3 - 9 mm

Chopped Strand

Technological properties

Property
Color

Brown

Other

Manufacturing Location: Canada

Processing history

Latex Type: SBR, Dip Pick-Up: 17 to 23%