Chloroprene latex impregnated E glass cord (Elastomer Polymer Matrix Composite)
Adhesion
Fad343 N at 20 °C
min., T Test
Linear density
ρlinear0.06 - 0.07 g/cm at 20 °C
Loss on Ignition
LOI16 - 22 % at 20 °C
Bobbin Inner Diameter
db,i57 - 63 mm
tapered
Bobbin Length
lb341 mm
Diameter
d2.32 - 2.62 mm
Apparent Diameter
Flange Diameter
Df279.5 mm
Color
Black
Cord Construction
140.3/12
Other
Manufacturing Location: UK / Poland
Processing history
Latex Type: Chloroprene
Twist per Meter
TPM28 - 51 TPM
Direction: S & Z
This material data has been provided by NGF Glass.