Glass cord 615/616 (D)

Alternative and trade names
Glass Cord
Want to keep this datasheet? Save it now in your required format

Description

Chloroprene latex impregnated E glass cord (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

59 N

Show Supplier Material materials with Adhesion of 59 N

min., T Test

Linear density

23.0 °C

1.2E-3 - 1.5E-3 g/cm

Show Supplier Material materials with Linear density of 1.2E-3 - 1.5E-3 g/cm

Loss on Ignition

23.0 °C

16.2 - 22.2 %

Show Supplier Material materials with Loss on Ignition of 16.2 - 22.2 %

Dimension

PropertyValueComment

Bobbin Inner Diameter

57 - 64 mm

Show Supplier Material materials with Bobbin Inner Diameter of 57 - 64 mm

tapered

Bobbin Length

305 mm

Show Supplier Material materials with Bobbin Length of 305 mm

Diameter

0.26 - 0.4 mm

Show Supplier Material materials with Diameter of 0.26 - 0.4 mm

Apparent Diameter

Flange Diameter

152.5 mm

Show Supplier Material materials with Flange Diameter of 152.5 mm

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.7 - 3.7 %

Show Supplier Material materials with Elongation of 1.7 - 3.7 %

Nominal breaking force

23.0 °C

59 N

Show Supplier Material materials with Nominal breaking force of 59 N

Tensile Member: E Glass

Technological properties

Property
Color

Black

Cord Construction

34.3/0

Other

Manufacturing Location: UK / Poland

Processing history

Latex Type: Chloroprene

Twist per Meter

130 - 154 TPM

Direction: S & Z